As mentioned in the fist tutorial, for the second installment of my 4 processes/projects a month (4PAM) is about how to keep kinetic metal clay components from fusing together in the kiln. If you aren't familiar with metal clay, in order for the clay to sinter, burn off the binder, and become solid metal, the temperature will range from 1100F to 1800F. Often this means touching components won't move after firing, or the surfaces where they were touching will be marred. This simple solution…